Mechanical Properties Metric English Comments
Peel Strength 13.1 kN/m

@Temperature 22.2 °C
75.0 pli

@Temperature 72.0 °F
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and ..