Mechanical Properties Metric English Comments
Peel Strength 2.03 kN/m

@Temperature 23.0 °C
11.6 pli

@Temperature 73.4 °F
Aluminum, etched, Bell Peel, Cohesive/Adhesive Failure; ASTM D3167
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..