Mechanical Properties Metric English Comments
Peel Strength 10.5 kN/m

@Temperature 21.1 °C
60.0 pli

@Temperature 70.0 °F
Metal to Metal Peel, Redux 775 Liquid & Powder (P:L Ration = 1.3:1)
Hexcel® Redux® 775 Vinyl phenolic structural adhesive
Redux 775 was adopted as the world's first metal-to-metal bonding process to be officially approved for use in the manufacture of aircraft primary structures in 1943. It is available either as a fil..
Peel Strength 10.5 kN/m

@Temperature 23.0 °C
60.0 pli

@Temperature 73.4 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 10.5 kN/m

@Temperature 60.0 °C,
Time 605000 sec
60.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, Stainless Steel; AMS-S83318
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..
Peel Strength 10.5 kN/m

@Temperature 60.0 °C,
Time 605000 sec
60.0 pli

@Temperature 140 °F,
Time 168 hour
JRF/SW, Titanium; AMS-S83318
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..