Mechanical Properties Metric English Comments
Peel Strength 1.93 kN/m

@Temperature 82.0 °C
11.0 pli

@Temperature 180 °F
Aluminum, Bell Peel
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Peel Strength 1.93 kN/m

@Temperature 82.0 °C,
Time 14400 sec
11.0 pli

@Temperature 180 °F,
Time 4.00 hour
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..