Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.09 kN/m @Thickness 0.0508 mm |
6.20 pli @Thickness 0.00200 in |
IPC-TM-650 2.4.8 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |