Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 90.0 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |