Mechanical Properties Metric English Comments
Tensile Strength 86.2 MPa

@Temperature 23.0 °C
12500 psi

@Temperature 73.4 °F
ASTM D638
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..