Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 86.0 MPa @Temperature 25.0 °C |
12500 psi @Temperature 77.0 °F |
ASTM D 638 |
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat.. |