Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.87 MPa @Strain 100 % |
851 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Tensile Strength | 5.87 MPa @Strain 100 % |
851 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Elastamax™ HTE 3170 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |