Tensile Strength 565 MPa

@Thickness 25.0 - 60.0 mm
81900 psi

@Thickness 0.984 - 2.36 in
Typical Strength
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..