Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 552 - 655 MPa @Thickness >=25.4 mm |
80000 - 95000 psi @Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |