Mechanical Properties Metric English Comments
Tensile Strength >= 530 MPa

@Thickness 25.0 - 50.0 mm
>= 76900 psi

@Thickness 0.984 - 1.97 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength 530 MPa

@Thickness 150 - 240 mm
76900 psi

@Thickness 5.91 - 9.45 in
Tempers T651 / T652
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Tensile Strength >= 530 MPa

@Thickness 25.0 - 50.0 mm
>= 76900 psi

@Thickness 0.984 - 1.97 in
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength 530 MPa

@Thickness 100 - 120 mm
76900 psi

@Thickness 3.94 - 4.72 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength >= 530 MPa

@Thickness 50.0 - 60.0 mm
>= 76900 psi

@Thickness 1.97 - 2.36 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..