Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 70.0 MPa @Temperature 50.0 °C |
10200 psi @Temperature 122 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Strength | 70.0 MPa @Strain 1.00 %, Temperature 60.0 °C |
10200 psi @Strain 1.00 %, Temperature 140 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |