Polymer Property : Tensile Strength = 64.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 64.0 MPa

@Temperature 150 °C
9280 psi

@Temperature 302 °F
ISO 527
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..