Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 43.4 MPa @Temperature 23.0 °C |
6290 psi @Temperature 73.4 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |