Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 430 MPa @Thickness 127 - 152.4 mm |
62400 psi @Thickness 5.00 - 6.000 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | >= 430 MPa @Thickness 400 - 450 mm |
>= 62400 psi @Thickness 15.7 - 17.7 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength | >= 430 MPa @Thickness 400 - 450 mm |
>= 62400 psi @Thickness 15.7 - 17.7 in |
Temper T652 |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |