Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.00 MPa @Strain 20.0 %, Temperature 50.0 °C |
870 psi @Strain 20.0 %, Temperature 122 °F |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |