Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 380 MPa @Thickness 152.4 - 203.2 mm |
>= 55100 psi @Thickness 6.000 - 8.000 in |
Tempers T851/T852) |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |