Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 48.3 MPa @Temperature 77.0 °C |
7010 psi @Temperature 171 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 48.3 MPa @Temperature 90.0 °C |
7000 psi @Temperature 194 °F |
ASTM D638 |
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin.. |