Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 45.0 MPa @Strain 2.00 %, Temperature 150 °C |
6530 psi @Strain 2.00 %, Temperature 302 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |