Polymer Property : Tensile Strength = 41.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 41.4 MPa

@Temperature 77.0 °C
6000 psi

@Temperature 171 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Tensile Strength 41.4 MPa

@Temperature 130 °C
6000 psi

@Temperature 266 °F
ASTM D638
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide
Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe..