Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 280 MPa @Diameter 40.0 - 80.0 mm |
40600 psi @Diameter 1.57 - 3.15 in |
|
United Cast Bar Unibar 350 Continuously Cast Iron Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a.. |