Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.00 MPa @Strain 20.0 %, Temperature 100 °C |
580 psi @Strain 20.0 %, Temperature 212 °F |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |