Polymer Property : Tensile Strength = 355 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 355 MPa

@Thickness 203.2 - 254 mm
>= 51500 psi

@Thickness 8.000 - 10.0 in
Tempers T851/T852)
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..