Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 240 MPa @Diameter 40.0 - 80.0 mm |
34800 psi @Diameter 1.57 - 3.15 in |
|
United Cast Bar Unibar 300 Continuously Cast Iron Unibar 300 is alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and an excellent surface finish.. |