Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 320 MPa @Thickness 254 - 305 mm |
>= 46400 psi @Thickness 10.0 - 12.0 in |
Tempers T851/T852) |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength | 320 MPa @Thickness 4.00 - 8.00 mm |
46400 psi @Thickness 0.157 - 0.315 in |
Typical Strength; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | 320 MPa @Thickness 60.0 - 150 mm |
46400 psi @Thickness 2.36 - 5.91 in |
Typical Strength; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | 320 MPa @Thickness 60.0 - 150 mm |
46400 psi @Thickness 2.36 - 5.91 in |
Typical Strength |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |