Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 31.0 MPa @Temperature 260 °C |
4500 psi @Temperature 500 °F |
ASTM D638 |
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin.. |
|||
Tensile Strength | 31.0 MPa @Strain 20.0 %, Temperature 70.0 °C |
4500 psi @Strain 20.0 %, Temperature 158 °F |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |