Tensile Strength 27.6 MPa

@Temperature 260 °C
4000 psi

@Temperature 500 °F
ASTM D638
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide
Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® ..