Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 168 MPa @Temperature 23.0 °C |
24400 psi @Temperature 73.4 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |