Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 207 MPa @Temperature 21.1 °C |
>= 30000 psi @Temperature 70.0 °F |
|
H.C. Starck NRC® Tantalum (UNS R05200) Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di.. |