Mechanical Properties Metric English Comments
Tensile Strength 142 MPa

@Temperature 23.0 °C
20600 psi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8556 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform..