Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 180 MPa @Diameter 20.0 - 40.0 mm |
26100 psi @Diameter 0.787 - 1.57 in |
|
United Cast Bar Unibar 200 Continuously Cast Iron Offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.Unibar-200 is not suitable for hard.. |
|||
Tensile Strength | 180 MPa @Temperature 70.0 °C, Time 180000 sec |
26100 psi @Temperature 158 °F, Time 50.0 hour |
62% RH |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Strength | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |