Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 114 MPa @Temperature -40.0 °C |
16500 psi @Temperature -40.0 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 114 MPa @Temperature -40.0 °C |
16500 psi @Temperature -40.0 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |