Tensile Strength 106 MPa

@Temperature 150 °C
15400 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8212 Polyimide
DuPont Vespel TP-8212 parts are specified for high-temperature applications requiring electrical insulation. TP-8212 parts offer a unique balance of mechanical and thermal properties with a low coef..
Tensile Strength 106 MPa

@Temperature 150 °C
15400 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8556 Polyimide