Polymer Property : Tensile Strength = 1500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 10.3 MPa

@Temperature 121 °C,
Time 605000 sec
1500 psi

@Temperature 250 °F,
Time 168 hour
Air Oven
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables..