Polymer Property : Tensile Strength = 144 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 144 MPa

@Temperature 150 °C
20900 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8474 Polyimide
DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation..