Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1410 MPa @Temperature -5.56 °C |
205000 psi @Temperature 22.0 °F |
45 HRC |
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |