Polymer Property : Tensile Strength = 138 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 138 MPa

@Temperature 23.0 °C
20000 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers