Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.00 MPa @Strain 20.0 %, Temperature 100 °C |
145 psi @Strain 20.0 %, Temperature 212 °F |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |