Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 14.6 kJ/m² @Temperature 0.000 °C |
6.95 ft-lb/in² @Temperature 32.0 °F |
Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-35 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Izod Impact, Unnotched (ISO) | 14.6 kJ/m² @Temperature 0.000 °C |
6.95 ft-lb/in² @Temperature 32.0 °F |
Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-56 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Izod Impact, Unnotched (ISO) | 14.6 kJ/m² @Temperature 0.000 °C |
6.95 ft-lb/in² @Temperature 32.0 °F |
Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Izod Impact, Unnotched (ISO) | 14.6 kJ/m² @Temperature 0.000 °C |
6.95 ft-lb/in² @Temperature 32.0 °F |
Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |