Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Izod Impact, Unnotched (ISO) | 13.0 kJ/m² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers |