Polymer Property : Izod Impact, Unnotched (ISO) = 220 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 220 kJ/m²

@Temperature -40.0 °C
105 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1U
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT  (Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
Izod Impact, Unnotched (ISO) 220 kJ/m²

@Temperature -30.0 °C
105 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT  (Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..