Izod Impact, Unnotched (ISO) 22.5 kJ/m²

@Temperature 0.000 °C
10.7 ft-lb/in²

@Temperature 32.0 °F
Phr = 8
Shandong Rike Chemical ACM-3A PVC Impact Modifier ACM Resin
Outline of ACM ResinFor overcoming the shortcomings of plasticizers and CPE, we developed a new type impact modifier ACM which as a copolymer of HDPE and acrylic acid and our ACM not only has the ba..