Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 180 kJ/m² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |