Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 17.0 kJ/m²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled
SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In..