Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 24.2 kJ/m² @Temperature 23.0 °C |
11.5 ft-lb/in² @Temperature 73.4 °F |
Phr = 5 |
Shandong Rike Chemical ACM-3 PVC Impact Modifier ACM Resin Outline of ACM ResinFor overcoming the shortcomings of plasticizers and CPE, we developed a new type impact modifier ACM which as a copolymer of HDPE and acrylic acid and our ACM not only has the ba.. |
|||
Izod Impact, Unnotched (ISO) | 24.1 kJ/m² @Temperature 0.000 °C |
11.5 ft-lb/in² @Temperature 32.0 °F |
Phr = 8 |
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |