Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0441 GPa

@Temperature 816 °C
6.40 ksi

@Temperature 1500 °F
Hot
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable
Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol..