Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0440 GPa | 6.38 ksi | EN 993-6: 1995 |
Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick Silicon nitride-bonded silicon carbide brick has the following characteristics: Max. service temperature 1580°C (2876°F)For sidewall lining of aluminum reduction cellsHigh thermal conductivity.. |