Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0438 GPa @Temperature 816 °C |
6.35 ksi @Temperature 1500 °F |
Hot |
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an.. |