Mechanical Properties Metric English Comments
Modulus of Rupture 0.0300 GPa

@Treatment Temp. 954 °C
4.35 ksi

@Treatment Temp. 1750 °F
fired and cooled
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable
Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol..
Modulus of Rupture 0.0300 GPa
4.35 ksi
parallel to thickness
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul..
Modulus of Rupture 0.0300 GPa
4.35 ksi
parallel to thickness
Zircar Refractory Composites RSLE-57 Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl..
Modulus of Rupture 0.0300 GPa

@Treatment Temp. 954 °C
4.35 ksi

@Treatment Temp. 1750 °F
fired and cooled
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable
Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an..